Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax TYC1175P G01 BLACK is a very high melt-flow, UV stabilized TPO compound typically used for automotive applications. Applications: Automotive Parts. Information provided by LyondellBasell. |