MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ovako 20MnCrS5 4324 Steel, Hot forging
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: General Information: Case-hardening steel with low carbon content but good hardenability reaching good wear resistance due to high surface hardness after hardening. The small grain size benefits in good ductility and fatigue strength. Suitable for gearboxes and axle gears.

Information provided by Ovako

Key Words: 1.7149, SAE 5120, AISI 4820, DIN 20MnCrS5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 270
@Thickness 25.0 - 160 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 385 °CMS
 731 °CAC1
 831 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.017 - 0.030 %
Carbon, C 0.17 - 0.20 %
Chromium, Cr 1.0 - 1.3 %
Iron, Fe 96.44 - 97.49 %As Balance
Manganese, Mn 1.0 - 1.25 %
Molybdenum, Mo 0.050 - 0.070 %
Nickel, Ni 0.10 - 0.25 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.15 - 0.40 %
Sulfur, S 0.025 - 0.040 %
 
Descriptive Properties
WeldabilityCEV 0.66max
 Pcm 0.34max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako 20MnCrS5 4326 Steel, Annealing
Ovako 20MnCrS5 4326 Steel, Hot forging
Ovako 20MnCrS5 4324 Steel, Annealing
Ovako 20MnCr5:EN10084 Steel
AISI 4118 Steel, direct quenched from pot, carburized, 230°C (450°F) temper

NOVAKO141 / 234440

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.