MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Nihon Superior SN100C3 High Temperature Dipper and Tinning Solder
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 227 - 310 °C
Solidus 227 °C
Liquidus 310 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 3.0 %
Germanium, Ge <= 0.010 %
Nickel, Ni 0.050 %
Tin, Sn 97 %As Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nihon Superior SN100C4 High Temperature Dipper and Tinning Solder
Nihon Superior SN100C Lead-Free Solder Alloy
Nihon Superior SN100CL Lead-Free Solder Alloy
Nihon Superior 95A Sn-Sb Lead-Free Solder Alloy
Nihon Superior SN96 Lead-Free Solder Alloy

NNSUPE992 / 120807

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.