MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Udel® P-3700 HC Polysulfone (PSU)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aesthetics for applications where a yellow cast is undesirable.

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Good Chemical Resistance; Good Toughness; High Clarity; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable

Uses: Appliance Components; Appliances; Decorative Parts; Electrical/Electronic Applications; Food Service Applications; Medical/Healthcare Applications; Optical Applications; Safety Equipment

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.18 mm
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 343 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.8 MPaASTM D638
Elongation at Break 45 %ASTM D638
Elongation at Yield 5.8 %ASTM D638
Tensile Modulus 2690 MPaASTM D638
Flexural Yield Strength 117 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.18 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
Deflection Temperature at 1.8 MPa (264 psi) 178 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 185 °CASTM E1356
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.635ASTM D542
Haze 2.0 %
@Thickness 2.54 mm
ASTM D1003
Yellow Index 2.0 %
@Thickness 2.54 mm
ASTM D1925
Transmission, Visible 77 - 83 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 149 °CHopper
Melt Temperature 329 - 385 °C
Mold Temperature 121 - 163 °C
Drying Temperature 149 °C
@Time <=12600 sec
Shot Size 50 - 75 %
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorColorless
FormPellets
Processing TechniqueExtrusion; Injection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Udel® P-1835 Polysulfone (PSU)
Avient Edgetek® PF-1000 Polysulfone
Westlake Plastics Thermalux® Film Made from UDEL® Polysulfone Resin
Ensinger TECASON™ S Polysulfone (PSU)
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)

PSOL8Y7379 / 177110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.