Impact Copolymer Applications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions such as corrugated board. Formolene 6501A is a medium impact copolymer with an excellent balance of toughness and stiffness. It is suited for blow molded bottles and containers, blown and cast film applications, and profile extrusions. Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA. |