MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Redwood Plastics REDCO™ LOAD+™ Fiber reinforced rubber pads
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Overview: DYNAMEX™ LOAD+™ fiber reinforced rubber pads are structural bearings with higher stiffness (see Figure 4). They are commonly used in applications involving higher load requirements and less rotational needs. Consisting of high-strength, weather resistant elastomers and vulcanized with synthetic reinforcing fibres, our pads are designed for structural projects with typical design loads of 2000psi.

Applications: DYNAMEX™ LOAD+™ is widely used in pre-cast concrete structural applications. Examples include beams, Tees, hollow core slabs or girders in precast and prestressed concrete structures such as parking garages, pedestrian overpasses, masonry pads and many more.

Product Details: Stocked from 3/8” thickness through to 1” thickness, DYNAMEX™ LOAD+™ pads can be supplied in full sheet, strips or cut-to-size. The material can be moulded and fully fabricated to meet additional requirements. Table 5 displays the material properties for these pads.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D 297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70 - 80ASTM D 2240
 65 - 85
Tensile Strength 6.30 - 7.70 MPaASTM D 412, Die C
 5.75 - 8.75 MPa
@Temperature >=70.0 °C,
Time 252000 sec
ASTM D 573
Elongation at Break >= 40 %Ultimate; ASTM D 412
 30 - 50 %
@Temperature >=70.0 °C,
Time 252000 sec
Ultimate; ASTM D 573
Compressive Strength 14500 psiASTM D 412
Tear Strength >= 70.1 kN/mASTM D 624, Die B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW100 / 296666

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.