MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Indium Corp. #1210 Battery Flux
Categories: Fluid

Material Notes: Features
  • Wide process window
  • Low fuming
  • Minimal residue
  • Minimizes corrosion

#1210 Battery Flux was specially formulated for high volume cast-on-strap manufacturing where rapid evaporation of solvent is necessary. This flux contains no chlorides, heavy metals or organic acids, which could affect the long term life of the batteries. #1210 Battery Flux provides excellent metallurgical fusing of all lead-based battery alloys as employed in the cast-on-strap process systems. #1210 Battery Flux exhibits very low fuming or smoke during process of manufacturing. This flux leaves very minimal residue after the burn-in process.

Characteristics:

  • Color - yellow
  • Odor - Alcoholic

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity  1.045 g/cc
@Temperature 15.5 °C
1.045 g/cc
@Temperature 59.9 °F
 1.104 g/cc
@Temperature 25.0 °C
1.104 g/cc
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 29.4 °C85.0 °FTCC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NNIN915 / 131554

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.