MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTATRON® PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes:
  • High heat deflection temperature
  • High flame retardant
  • Very low smoke development
Product applications:
  • Electrical industry
  • Medical engineering
  • Aircraft construction

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.030 %0.030 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Hardness, Rockwell R 125125ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength, Yield 89.6 MPa13000 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 3.31 GPa480 ksiASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
Flexural Modulus 3.96 GPa575 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Shear Strength 62.1 MPa9000 psiASTM D732
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 21.3 kV/mm541 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.4 µm/m-°C28.0 µin/in-°FASTM D696
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°F
Melting Point 279 °C535 °FASTM D789
Maximum Service Temperature, Air 218 °C425 °F
Deflection Temperature at 0.46 MPa (66 psi) 204 °C400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNo
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9066 / 232769

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.