MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Oppalyte™ 52MH647 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Low sealing threshold
  • High seal strengths even under low pressure sealing
  • Good aroma barrier
  • Excellent packaging machine performance
  • Outstanding opacity, white background and reduced show-through
  • Excellent stiffness
  • Ideal support for normal ink systems
  • Water based coatings
Features:
  • Acrylic Coating
  • Flavor & Aroma Barrier
  • Light Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crisps and Snacks
  • Dry Foods and Beverage Powders
  • Health and Beauty Care
  • Household and Detergents
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print Unsupported

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 90.0 %90.0 %Whiteness Index
Water Vapor Transmission  0.497 g/m²/day
@Temperature 23.0 °C
0.0320 g/100 in²/day
@Temperature 73.4 °F
85% RH; ExxonMobil Method
 2.95 g/m²/day
@Temperature 38.0 °C
0.190 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate  650 cc/m²/day
@Temperature 23.0 °C
41.9 cc/100 in²/day
@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
 652 cc/m²/day
@Temperature 23.0 °C
42.0 cc/100 in²/day
@Temperature 73.4 °F
0% RH; ExxonMobil Method
Thickness 50.8 microns2.00 milExxonMobil Method
Coating Weight 37.9 g/m²23.7 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 170 %170 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 55 %55 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 1.70 GPa247 ksiMD; ExxonMobil Method
 2.80 GPa406 ksiTD; ExxonMobil Method
Coefficient of Friction 0.250.25Both Sides; ExxonMobil Method
Seal Strength 610 g/25 mm
@Pressure 0.276 MPa,
Temperature 130 °C
610 g/in
@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.5 sec; ExxonMobil Method
Film Tensile Strength at Break, MD 105 MPa15200 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 185 MPa26800 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.0 %
@Temperature 135 °C,
Time 432 sec
4.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 2.0 %
@Temperature 135 °C,
Time 432 sec
2.0 %
@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Gloss 70 %70 %45°; ExxonMobil Method
Transmission, Visible 22 %22 %ExxonMobil Method
 
Descriptive Properties
Yield18300 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Glass Fiber Filler
ExxonMobil Oppalyte™ 52MH648 OPP Film
ExxonMobil Oppalyte™ 50MO747 OPP Film
ExxonMobil Oppalyte™ 245STW-RH OPP Film
ExxonMobil Oppalyte™ 245ICN OPP Film

PEX99521 / 175757

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.