MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon™ Type C-20, both sides cementable FEP Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Teflon™ FEP film is a transparent, thermoplastic film that can be heat sealed, thermoformed, vacuum formed, heat bonded, welded, metalized, and laminated to many other materials, as well as used as an excellent hot-melt adhesive. This wide variety of fabrication possibilities combines with the following important properties to offer a unique balance of capabilities not available in any other plastic film: Chemical Compatibility, Electrical Reliability, Wide Thermal Range, Mechanical Toughness, Long Time Weather ability, and Reliability.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 g/cc0.0777 lb/in³ASTM D1505
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Moisture Absorption <= 0.0100 %<= 0.0100 %
Specific Surface Area 0.0038 m²/g0.0038 m²/g
 0.0090 m²/g0.0090 m²/g
 0.018 m²/g0.018 m²/g
Water Vapor Transmission 6.21 g/m²/day0.400 g/100 in²/dayASTM E96
Oxygen Transmission 11600 cc-mm/m²-24hr-atm29500 cc-mil/100 in²-24hr-atmASTM D1434
Nitrogen Transmission 5000 cc-mm/m²-24hr-atm12700 cc-mil/100 in²-24hr-atmASTM D1434
Carbon Dioxide Transmission 25900 cc-mm/m²-24hr-atm65800 cc-mil/100 in²-24hr-atmASTM D1434
Hydrogen Sulfide Transmission 34100 cc-mm/m²-24hr-atm86600 cc-mil/100 in²-24hr-atmASTM D1434
Permeability 0.310.31Carbon Tetrachloride. g/100 in2·24 hr.; ASTM E96
 0.410.41Acetic Acid. g/100 in2·24 hr.; ASTM E96
 0.560.56Hexane. g/100 in2·24 hr.; ASTM E96
 0.640.64Benzene. g/100 in2·24 hr.; ASTM E96
 0.690.69Ethyl Alcohol. g/100 in2·24 hr.; ASTM E96
 0.950.95Acetone. g/100 in2·24 hr.; ASTM E96
Thickness 25.4 microns1.00 mil
 50.8 microns2.00 mil
 127 microns5.00 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength at Break 20.7 MPa3000 psiASTM D882
Tensile Strength 23.0 MPa3340 psiASTM D1457
Tensile Strength, Yield 12.0 MPa1740 psiASTM D882
Elongation at Break 300 %300 %ASTM D882
Modulus of Elasticity 0.483 GPa70.0 ksiASTM D882
Flexural Modulus 0.586 GPa85.0 ksiASTM D790
Flex Crack Resistance 1000010000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched 76.9 J/cm144 ft-lb/inChemours pneumatic impact tester
Coefficient of Friction 0.10 - 0.300.10 - 0.30ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm
@Temperature -40.0 - 240 °C
>= 1.00e+18 ohm-cm
@Temperature -40.0 - 464 °F
ASTM D257
Surface Resistivity per Square >= 1.00e+16 ohm
@Temperature -40.0 - 240 °C
>= 1.00e+16 ohm
@Temperature -40.0 - 464 °F
ASTM D257
Insulation Resistivity  19800 Megaohm/1000 m
@Temperature 200 °C
65000 Megaohm/1000 ft
@Temperature 392 °F
0.2 MF wound capacitor section, single layer, Teflon™ 50A film.
 76200 Megaohm/1000 m
@Temperature 150 °C
250000 Megaohm/1000 ft
@Temperature 302 °F
0.2 MF wound capacitor section, single layer, Teflon™ 50A film.
 107000 Megaohm/1000 m
@Temperature 100 °C
350000 Megaohm/1000 ft
@Temperature 212 °F
0.2 MF wound capacitor section, single layer, Teflon™ 50A film.
Dielectric Constant  1.93 - 2.02
@Frequency 1000 Hz,
Temperature -40.0 - 225 °C
1.93 - 2.02
@Frequency 1000 Hz,
Temperature -40.0 - 437 °F
ASTM D150
 2.0
@Frequency 100 - 1.00e+6 Hz,
Temperature 25.0 °C
2.0
@Frequency 100 - 1.00e+6 Hz,
Temperature 77.0 °F
ASTM D150
Dielectric Strength  70.0 kV/mm
@Thickness 0.500 mm
1780 kV/in
@Thickness 0.0197 in
Short-time, in air; ASTM D149 Method A
 260 kV/mm
@Thickness 0.0250 mm
6600 kV/in
@Thickness 0.000984 in
Short-time, in air; ASTM D149 Method A
Dissipation Factor  0.00020
@Frequency 1000 Hz,
Temperature -40.0 - 225 °C
0.00020
@Frequency 1000 Hz,
Temperature -40.0 - 437 °F
ASTM D150
 0.00020 - 0.00070
@Frequency 100 - 1.00e+6 Hz,
Temperature 25.0 °C
0.00020 - 0.00070
@Frequency 100 - 1.00e+6 Hz,
Temperature 77.0 °F
ASTM D150
 0.00050
@Frequency 1e+6 Hz,
Temperature -40.0 - 240 °C
0.00050
@Frequency 1e+6 Hz,
Temperature -40.0 - 464 °F
ASTM D150
Arc Resistance >= 165 sec>= 165 secSamples melted in arc did not track.; ASTM D495
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 0.195 W/m-K1.35 BTU-in/hr-ft²-°FCenco-Fitch
Melting Point 260 - 280 °C500 - 536 °FDTA; ASTM D3418
Maximum Service Temperature, Air 255 °C491 °FZero Strength Temperature
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FD648 Tensile Bars
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C124 °FD648 Tensile Bars
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.341 - 1.3471.341 - 1.347
Transmission, Visible 96 %96 %Solar Transmission; ASTM E-424
 
Descriptive Properties
Bursting Strength (Mullen)11 psiASTM D774
Chemical/Solvent ResistanceExcellentASTM D543
Detergent Resistance (hours)480On grit blast aluminum
 600On aluminum
 744
Dimensional Stability0.72% ExpanseMD. 30 minutes at 150°C
 2.2% shrinkageTD. 30 minutes at 150°C
Flammability RatingVTM-O
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Tear Strength-Initial (Graves)270 g forceASTM D1004
Tear Strength-Propagating (Elmendorf)125 gASTM D 1922
Weather Resistance (years unaffected)20No adverse effects. Continuous exposure in Florida.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8845 / 268772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.