MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plastcom SLOVAMID 6 GB 20 Polyamide 6, 20% Glass Beads
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Features

Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properties, these can be modified by addition of GF, as a result of which the anisotropy is worsened. PA 6 for injection moulding, reinforced with 20% glass beads offers high grade surface brightness, low rolling resistance force. Application: throttle valves for air piping. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0154 cm/cm0.0154 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0165 cm/cm0.0165 in/inSTN 64 0808
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiSTN EN ISO 527-2
Elongation at Break 20 %20 %STN EN ISO 527-2
Tensile Modulus 3.30 GPa479 ksiSTN EN ISO 527-2
Flexural Strength 85.0 MPa12300 psiSTN EN ISO 178
Flexural Modulus 2.80 GPa406 ksiSTN EN ISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 4.50 J/cm²
@Temperature -20.0 °C
21.4 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  0.150 J/cm²
@Temperature -20.0 °C
0.714 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 0.250 J/cm²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FSTN EN ISO 75/A
Vicat Softening Point 200 °C392 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACO035 / 106913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.