MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAFLEX H / SPA2 60 A.05 SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: TPE-S, Shore A60, modified for good adhesion to polyamides such as PA6, PA66, PA6.12 or partially aromatic PA grades such as GRIVORY GV or GRIVORY HT (manufacturer EMS-GRIVORY)

Properties: flexible, good haptics, adhesion modified, semi-crystalline, soft

Typical areas of application: Sealing elements, Seals, Handles, Haptic components

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Mechanical Engineering, Furniture industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.0130 cm/cm0.0130 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0110 cm/cm0.0110 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60.060.0DIN ISO 7619-1
Tensile Strength at Break 5.10 MPa740 psiISO 527-1
Tensile Strength, Yield 0.600 MPa
@Strain 10.0 %
87.0 psi
@Strain 10.0 %
DIN EN ISO 527-1
Elongation at Break 750 %750 %ISO 527-1
50% Modulus 1.30 MPa
@Strain 50.0 %
1.30 MPa
@Strain 50.0 %
DIN EN ISO 527-1
100% Modulus 1.80 MPa
@Strain 100 %
261 psi
@Strain 100 %
DIN EN ISO 527-1
300% Modulus 2.80 MPa
@Strain 300 %
406 psi
@Strain 300 %
DIN EN ISO 527-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO596 / 326670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.