MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röchling Glastic Laminates/Shapes 1603-2D Fiberglass-Reinforced Polyester Standoff Insulator
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Crush Resistance 9070 kg20000 lb (mass)Compressive Strength
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 180 sec180 sec
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 130 °C266 °F
UL RTI, Mechanical with Impact 130 °C266 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Tensile Strength2500 lbs.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes 1603-2A Fiberglass-Reinforced Polyester Standoff Insulator
Röchling Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod
Röchling Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester
Röchling Glastic 4640-15 Fiberglass-Reinforced Polyester Standoff Insulator
Röchling Glastic 4610-10-E Fiberglass-Reinforced Polyester Standoff Insulator

PGLASO / 41925

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.