MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Saint-Gobain CHR® 2925-11 Glass-Foil Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2925 and 2995-11R are manufactured from aluminium foil laminated to fibreglass cloth with high-temperature silicone adhesive on one side.

Features/Benefits: CHR® 2925’s high-temperature silicone adhesive allows the product to withstand continuous high temperatures, and prevents tape slippage after application. CHR® 2995-11R is formed by laminating 0.127 mm, dead soft aluminium foil to fibreglass fabric and applying a special blend of high-temperature silicone adhesives. The backing provides an excellent combination of strength, flexibility and heat resistance. Both 2925 and 2995-11R have excellent strength and flexibility, which provides easy wrapping of complex shapes and minimizes wrinkling.

Applications: CHR® 2925 performs as a plasma or flame spray masking tape, allowing areas to be free of grit blasting and the plasma spray coating. Its high-temperature resistance makes it ideal for heat and reflectant tapes, and it is used in aerospace and automotive markets as a wire harness bundling tape in engine components. CHR® 2925 also is used as a sound and vibration dampening product. CHR® 2995-11R is designed for extremely high demand thermal spray applications, such as HVOF and High Detonation Systems. It provides excellent abrasion and temperature resistance and conforms very well to a wide variety of surface configurations. The extremely aggressive adhesive system assures the tape stays in place throughout the entire coating process and will release cleanly after use, reducing the cleaning of the coated parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 7.0 %7.0 %
Tear Strength 34.3 kN/m196 pliTensile Strength
Peel Strength 0.820 kN/m4.68 pliAdhesion to Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Descriptive Properties
ColorAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ387 / 68901

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.