DuPure G 01 NP is a non-pelletized polypropylene homopolymer (produced with a phthalate-free catalyst) supplied in the form of unstabilized free flowing powder. The spherical shape and narrow particle size distribution (with low fines content) makes DuPure G 01 NP very suitable for mixing with additives, fillers and color pigments/concentratesInformation provided by Carmel Olefins Ltd. |