MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Braskem HDF1050 High molecular weight high density polyethylene copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: HDF1050 is a high molecular weight high density polyethylene copolymer with broad bimodal weight distribution developed for the blown film segment. Films made with this resin offer high stiffness, good heat sealing response and resistance to trait propagation.
Applications: Very thin film on high-speed line, low caliber.
Processes: Blown Film Extrusion.

Film properties tested with a monolayer 12 µm thickness blown film, blow up ratio: 4.5, die gap: 1.2 mm.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D792
ESCR 10% Igepal® >= 1000 hourCondition B; ASTM D1693
Melt Flow 0.060 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 9.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPaASTM D638
Tensile Strength, Yield 22.0 MPaASTM D882
 26.0 MPaASTM D638
Film Elongation at Break, MD 240 %ASTM D882
Film Elongation at Break, TD 380 %ASTM D882
Film Elongation at Yield, TD 6.0 %ASTM D882
Modulus of Elasticity 1.06 GPaASTM D638
Izod Impact, Unnotched 480 J/mASTM D256/A
Elmendorf Tear Strength TD 90 gASTM D1922
Dart Drop Test 220 gASTM D1709/A
Film Tensile Strength at Break, MD 60.0 MPaASTM D882
Film Tensile Strength at Break, TD 31.0 MPaASTM D882
1% Secant Modulus, MD 665 MPaASTM D882
1% Secant Modulus, TD 871 MPaASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRAS617 / 314010

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.