MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C64810, NKUNS C4820, H06 Temper, Sheet
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 648 - 848 MPa94000 - 123000 psi
 752 MPa109000 psiTypical
Tensile Strength, Ultimate 779 MPa113000 psiTypical
 683 - 883 MPa99000 - 128000 psiTypical, in Shear
Tensile Strength, Yield 20.7 MPa3000 psi
Tensile Modulus 120 GPa17400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 ohm-cm0.00000290 ohm-cm60% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 20.5 W/m-K142 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr <= 0.090 %<= 0.090 %
Cobalt, Co 0.50 - 3.0 %0.50 - 3.0 %
Copper, Cu 92.2 - 99.2 %92.2 - 99.2 %As Balance
Iron, Fe <= 1.0 %<= 1.0 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg <= 0.20 %<= 0.20 %
Nickel, Ni 0.10 - 1.0 %0.10 - 1.0 %
Phosphorus, P <= 0.50 %<= 0.50 %
Silicon, Si 0.20 - 1.0 %0.20 - 1.0 %
Tin, Sn <= 0.50 %<= 0.50 %
Zinc, Zn <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64810x1 / 292255

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.