MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KiON Pack B URETHANE HYBRID CLEAR COAT Heat-Curable Polysilazane-Based Hybrid Spray Coat  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: KiON Urethane Hybrid Clear Coat is a ready-to-use clear coat containing both polysilazane and polyurethane components that can be thermally-cured to provide an oxidation and corrosion-resistant clear or pigmented finish. KiON Urethane Hybrid Clear Coat is furnished as a 2-Pack system that can be applied by spray, dip, and brush coating techniques. It cures upon heating to temperatures of between 293 °F and 311 °F for 1 hour. KiON Urethane Hybrid Clear Coat provides a clear, protective coating for both ferrous and non-ferrous metals and alloys, ceramics, glass, etc. In addition, KiON Urethane Hybrid Clear Coat has excellent “weatherability”, UV resistance, hardness and abrasion resistance.

Applications

Clear, protective coatings for both ferrous and non-ferrous metals and alloys, clear automotive finishes, thermally durable coatings, and industrial, infrastructure and marine coatings.

Information provided by KiON Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9789 g/cc0.03537 lb/in³Liquid
Volatile Organic Compounds (VOC) Content 189 g/l189 g/l
Viscosity 4.1 cP
@Temperature 19.0 °C
4.1 cP
@Temperature 66.2 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 29.0 °C>= 84.2 °F
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %at 60 degrees
 
Descriptive Properties
%Resin52.7 wt% solids
AppearanceClear, colorless
Pencil Hardness ASTM D 33636H after thermal cure on aluminum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKION12 / 48728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.