Type: Aliphatic polycaprolactone based Thermoplastic Polyurethane (TPU) with a 90 Shore A Hardness. Features: Clear resin with excellent colour stability upon UV exposure. Uses: Cast film extrusion, profile extrusion. Information provided by The 159 Corporation |