MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teonex® Q72 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film. This ultra thin film which was developed for capacitor applications. It is commercially available in nominal 14 gauge (3.5 micron).

Approvals: UL Component Registration (RTI = 180/160°C) - Relative Thermal Index (RTI) = 180°C (Elect), 160°C (Mech)

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Thickness 3.56 microns0.140 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 74 %74 %ASTM D882-67 (Modified to TDF)
Film Elongation at Break, TD 73 %73 %ASTM D882-67 (Modified to TDF)
Coefficient of Friction, Dynamic 0.200.20ASTM D1894
Coefficient of Friction, Static 0.300.30ASTM D1894
Film Tensile Strength at Break, MD 255 MPa37000 psiASTM D882-67 (Modified to TDF)
Film Tensile Strength at Break, TD 276 MPa40000 psiASTM D882-67 (Modified to TDF)
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 330 kV/mm8380 kV/inJIS C-2319
 
Thermal PropertiesMetricEnglishComments
Melting Point 269 °C516 °FDSC
UL RTI, Electrical 160 °C320 °F
UL RTI, Mechanical without Impact 180 °C356 °F
Shrinkage, MD 1.0 %
@Temperature 150 °C
1.0 %
@Temperature 302 °F
JIS C-2318 (Modified to TDF)
Shrinkage, TD 1.3 %
@Temperature 150 °C
1.3 %
@Temperature 302 °F
JIS C-2318 (Modified to TDF)
 
Descriptive Properties
Surface Roughness0.074TDF Method (Inside)
 1.3TDF Method (Rm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge
DuPont Teijin Films Teonex® Q65FA
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness

PDTZ9498 / 139815

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.