Machine dispensed epoxy paste Key Properties: - Very dense, closed surface. Can be polished directly. No sealing necessary.
- Layer thickness 20 mm without slump on vertical surfaces
- Heat resistant up to 130°C after appropriate postcure
Applications: - Tools
- Molds for direct tooling
Cure: 10 h at 20-25°C + 14 h at 130°CInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |