MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® 15W-50 High Performance Synthetic Motor Oil
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Description: Conoco Syncon HP Synthetic Motor Oil is formulated for most domestic or imported vehicles with gasoline-powered engines. It works well at extreme temperatures and in severe driving conditions. The SAE 5W-30 and 10W-30 grades have ILSAC GF-2 energy-conserving credentials and carry the API certification mark for use in gasoline engines. All three viscosity grades (SAE 5W-30, 10W-30 and 15W-50) are approved for API Service SJ and CF. Syncon HP Synthetic Motor Oil is manufactured with premium synthetic PAO base stocks and offers excellent thermal and oxidative stability, minimum oil thickening at high-operating temperatures and outstanding control of deposits and wear at all temperatures. In the appropriate manufacturer-recommended viscosity grade, Syncon HP Synthetic Motor Oil meets these specifications:
  • Ford WSS-M2C153-G and WSS-M2C910-A1 and A2
  • Chrysler MS-6395H and MS-9615
  • GM 9986125, 9986126, and 9986137
  • ILSAC GF-2 (5W-30 and 10W-30 viscosity grades only)

The SAE 5W-30 and SAE 10W-30 viscosity grades also can be used as antiwear hydraulic fluid in mobile equipment and as a compressor oil where the manufacturer specifies a synthetic motor oil. The excellent antiwear properties and low-temperature fluidity of these oils suit them for use in hydraulic systems and compressors year-round.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.6 °
Viscosity Measurement 154Viscosity Index
Saybolt Viscosity at 100°F 596 SUS
Saybolt Viscosity at 210°F 83 SUS
Kinematic Viscosity at 40°C (104°F) 129 cSt
Kinematic Viscosity at 100°C (212°F) 18 cSt
ASTM Color 2.5
 
Thermal PropertiesOriginal ValueComments
Pour Point -55.0 °F
Flash Point 460 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kanthal® 52 Nickel-Iron Resistor Alloy
Dow 1500 Antifoam
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Sharadaa Ceramics LI SILL-I High Alumina Brick
Sharadaa Ceramics LI 50K High Alumina Brick

WCON040 / 75077

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.