MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 177.1520(c)(2.2) and may be used as a component of packages used for holding food during cooking.

Technical Data Sheet

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

Information provided by Eastman Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D4883
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 13.8 MPa500 mm/min (20 in./min); ASTM D638
Tensile Strength, Yield 11.0 MPa500 mm/min (20 in./min); ASTM D638
Elongation at Break 500 %500 mm/min (20 in./min); ASTM D638
Flexural Modulus 0.221 GPa
@Strain 2 %
Secant; ASTM D 790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °CASTM D1525
Brittleness Temperature -73.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman 1830A Polyethylene
Eastman 1830E Polyethylene
Arkema Orevac® 18302 Maleic Anhydride modified LLDPE
Eastman 1830F Polyethylene
Westlake EN1817AA Low Density Polyethylene

PEA225 / 35259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.