MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Epoxies, Etc 10-3784 One Component Epoxy Adhesive Series
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: These one component heat cure epoxy adhesives are fast setting materials formulated in three different viscosities. They are known for their low temperature cure, heat and excellent chemical resistance.
10-3782 Very low viscosity
10-3783 Medium viscosity
10-3784 Paste non-sag
These unique adhesives exhibit outstanding bond strengths to a variety of substrates including metals, ceramics, wood, magnets, plastics, glass, etc. They are currently used in a variety of electronic bonding and potting applications, filer end cap assemblies, magnetic bonding applications and anywhere a tough indestructible bond is required

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  70
@Temperature 121 °C
70
@Temperature 250 °F
 80
@Temperature 25.0 °C
80
@Temperature 77.0 °F
Tensile Strength 27.6 MPa4000 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 175 °C
0.0333 hour
@Temperature 347 °F
 5.00 min
@Temperature 160 °C
0.0833 hour
@Temperature 320 °F
 15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F
 120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
Shelf Life  6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
 12.0 Month
@Temperature 0.000 °C
12.0 Month
@Temperature 32.0 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX091 / 316768

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.