MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil Tin Catalyst Deep Section Catalyst
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: QSil Deep Section Catalyst can be used with two-component, room temperature, condensation cure silicone materials.

Key Features:

  • High durometer
  • Fast cure
  • Excellent dimensional stability
  • Deep section cure
Main Applications:
  • Potting and encapsulation of electronic components

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccUncatalyzed
Viscosity 6500 cPUncatalyzed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40Cured 24 hrs at RT
Tensile Strength 200 psiCured 24 hrs at RT
Elongation at Break 200 %Cured 24 hrs at RT
Tear Strength 20.0 pliCured 24 hrs at RT
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CCured 24 hrs at RT
Minimum Service Temperature, Air -55.0 °CCured 24 hrs at RT
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
Tack-Free Time 2.00 hourCatalyzed
Gel Time 70.0 minCatalyzed
 
Descriptive Properties
ColorBeigeUncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion WS145 Solder
Materion WS179 Solder
Materion WS181 Solder
Materion WS183 Solder
Materion WS186 Solder

PACC2112 / 199500

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.