MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Redwood Plastics CAN/CSA S6-19 Neoprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 6050 - 60ASTM D 2240
 <= 70
@Temperature >=100 °C,
Time 252000 sec
<= 70
@Temperature >=212 °F,
Time 70.0 hour
ASTM D 573
Tensile Strength >= 17.0 MPa>= 2470 psiASTM D412, Method A
 >= 14.45 MPa
@Temperature >=70.0 °C,
Time 360000 sec
>= 2096 psi
@Temperature >=158 °F,
Time 100 hour
ASTM D 573
Elongation at Break >= 400 %>= 400 %Ultimate; ASTM D412, Method A
 >= 240 %
@Temperature >=70.0 °C,
Time 360000 sec
>= 240 %
@Temperature >=158 °F,
Time 100 hour
ASTM D 573
Compression Set <= 25 %
@Temperature 70.0 °C,
Time 79200 sec
<= 25 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D 395 Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -40.0 °C-40.0 °FNo Failure at Temp; ASTM D746, Procedure B
 
Descriptive Properties
Bonding Strength>7 N.mm-1Bond Between Steel and Elastomer Laminae, ASTM D 429, Method B
Ozone ResistanceNo CracksASTM D 1149, Mounting Procedure A, 20% Strain , 40±2°C. 25 pphm, 48h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW095 / 296661

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.