MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huafon EP158 Nylon 66, Chips
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product Description: EP158 is a general purpose Nylon 66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength; good toughness; high impact; good surface lubricity; abrasion resistance; resistant low temperature; self-extinguishment.

Typical Applications: EP158 is suitable for compounding and injection molding, also widely used in spinning monofilament, staple. Terminal applications mainly in machinery, electronics, electrical, instrumentation, automotive components, railway, home appliances, communications, textile, oil pip/tank and precision engineering products, etc. EP158 also can be used for the production of film packing, medical equipment, sporting goods, and daily necessities and so on.

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2.62 - 2.72 cP
Melt Flow 71.2 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.3 MPa
@Time 173000 sec
50% RH; ISO 527
Elongation at Break 70.1 %
@Time 173000 sec
50% RH; ISO 527
Flexural Strength 99.6 MPa
@Time 173000 sec
50% RH; ISO 178
Flexural Modulus 2659 MPa
@Time 173000 sec
50% RH; ISO 178
Charpy Impact, Notched 6.10 kJ/m²
@Time 173000 sec
50% RH; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 267.5 °C10°C/min; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 185.5 °C
@Time 173000 sec
50% RH; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 67.4 °C
@Time 173000 sec
50% RH; ISO 75
Vicat Softening Point 239.7 °C
@Load 5.10 kg,
Time 173000 sec
120°C/h, 50% RH; ISO 306
Flammability, UL94 V-2
@Thickness 1.00 mm,
Time 173000 sec
50% RH
 V-2
@Thickness 1.60 mm,
Time 173000 sec
50% RH
 V-2
@Thickness 3.00 mm,
Time 173000 sec
50% RH
 
Descriptive Properties
AppearanceTransparent particle
NH236-46 mmol/kg
Particle size1.2-1.4 g/100 Pellets
Water content<5000 mg/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHUAF281 / 295224

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.