MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAFIL PC FR natural - 2,85 mm - Filament Polycarbonate, Flame Retardant
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes:
  • electrically insulating
  • good weldable and bondable
  • tested according to EN 45545
  • flame retardant as per FAR 25.853
  • flame retardant according to UL94 V-0
Target Industries:
  • electronics
  • Railway Interiors
  • automotive industry
  • mechanical engineering
  • aircraft and aerospace interiors
  • aircraft and aerospace technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Moisture Absorption 0.140 %DIN EN ISO 62
Melt Flow 35.3 g/10 min
@Load 1.20 kg,
Temperature 300 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 34.0 MPa5mm/min, Orientation ZX; DIN EN ISO 527-2
 69.0 MPa5mm/min, Orientation XY; DIN EN ISO 527-2
Elongation at Break 1.4 %5mm/min, Orientation ZX; DIN EN ISO 527-2
 3.8 %5mm/min, Orientation XY; DIN EN ISO 527-2
Modulus of Elasticity 2.75 GPa5mm/min, Orientation XY; DIN EN ISO 527-2
 2.80 GPa5mm/min, Orientation ZX; DIN EN ISO 527-2
Flexural Strength 67.0 MPa2mm/min, Orientation ZX; DIN EN ISO 178
 105 MPa2mm/min, Orientation XY; DIN EN ISO 178
Flexural Modulus 2750 MPa2mm/min, Orientation XY; DIN EN ISO 178
 3300 MPa2mm/min, Orientation ZX; DIN EN ISO 178
Flexural Strain at Break 1.8 %2mm/min, Orientation ZX; DIN EN ISO 178
 3.9 %2mm/min, Orientation XY; DIN EN ISO 178
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °Clong term
 70.0 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °CISO-R 75 Method A
Glass Transition Temp, Tg 80.0 °CASTM D3418
Flammability, UL94 V-0125x13x1,5mm; Orientation XY; DIN IEC 60695-11-10
 V-0125x13x5,0mm; Orientation XY; DIN IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °CPrint bed temperature
Nozzle Temperature 240 - 280 °CDiameter: 0,4 mm
Melt Temperature <= 300 °C
Drying Temperature 60.0 °C
Dry Time 8.00 hour
 
Descriptive Properties
Colornatural transparent
Fan speed (%)40
Flammability1.5 mm60 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(i)
 1.5 mm12 sec. Vertical Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(ii)
 1.5 mm15 sec. Horizontal Bunsen Burner test, FAR §25.853 (a) and Appendix F, Part I, para. (a)(1)(iv)
 1.5 mmGas Toxicity, as per Boeing BSS 7239
 R22 HL3, R23 HL3s=1,5mm & s=10mm; EN 45545-2:2016
Print speed30-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO1262 / 319190

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.