MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® R 865/70 HCR Silicone
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R 865/70 offers numerous functional advantages. The material ensures superior rebound resiliency and a minimal compression set. The compounds are easily pigmentable with ELASTOSIL® PT Pigment Pastes and have good processing characteristics. The various grades (ELASTOSIL® R 865/40 - ELASTOSIL® R 865/70) can be blended in any proportion to achieve intermediate hardnesses.

Application: ELASTOSIL® R 865/70 is especially designed for peroxide curing applications as

  • calendaring
  • molding

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccDIN 51757
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68DIN 53505
Tensile Strength 1320 psiDIN 53404 S1
Elongation at Break 320 %DIN 53404 S1
Rebound 55 %DIN 53512
Tear Strength 108 pliASTM D624 B
Compression Set 9.0 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 165 °C
0.5% ELASTOSIL® AUX Crosslinker C6; Post-Cured 4h/200 ºC
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® R 865/40 HCR Silicone
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker ELASTOSIL® R 407/70 Silicone Rubber Base
Polychloroprene Rubber (CR)
Overview of materials for Liquid Silicone Rubber

PWACK9919 / 197518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.