MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 4731-13 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability and UV resistance.

Applications:
  • Information Technology Equipment
  • Power Tools
  • Electrical Appliances and Parts

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Filler Content 10 %Glass; ASTM 5630B
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
Melt Flow 13 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength, Ultimate 9100 psi0.125 in, injection molded, unannealed; ASTM D638
Tensile Strength, Yield 9500 psi0.125 in, injection molded, unannealed; ASTM D638
Elongation at Break 4.0 %0.125 in, injection molded, unannealed; ASTM D638
Tensile Modulus 530000 psi0.125 in, injection molded, unannealed; ASTM D638
Flexural Strength 15800 psi0.125 in, injection molded, unannealed; ASTM D790
Flexural Modulus 550000 psi0.125 in, injection molded, unannealed; ASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 µin/in-°F
@Temperature -40.0 - 82.2 °C
ASTM D696
Hot Ball Pressure Test >= 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 300 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 275 °Fannealed; ASTM D648
 285 °Funannealed; ASTM D648
Vicat Softening Point 320 °F50°C/hr, 50N; ASTM D1525
UL RTI, Electrical 257 °FUL 746
UL RTI, Mechanical with Impact 221 °FUL 746
UL RTI, Mechanical without Impact 257 °FUL 746
Flammability, UL94 V-0
@Thickness 1.59 mm
 V-0
@Thickness 3.17 mm
Oxygen Index 38 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 288 - 316 °C
Mold Temperature 82.0 - 116 °C
Drying Temperature 121 °C
Dry Time 3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 4850-10 Polycarbonate

PZZDOW1362 / 30580

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.