MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Freudenberg Sealing Technologies Ventoguard 467 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc
@Temperature 23.0 °C
0.0455 lb/in³
@Temperature 73.4 °F
DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Temperature 23.0 °C
75
@Temperature 73.4 °F
DIN ISO 7619-1
Tensile Strength 20.0 MPa
@Temperature 23.0 °C
2900 psi
@Temperature 73.4 °F
DIN 53504, S2
Elongation at Break 306 %
@Temperature 23.0 °C
306 %
@Temperature 73.4 °F
DIN 53504, S2
100% Modulus 7.00 MPa
@Temperature 23.0 °C
1020 psi
@Temperature 73.4 °F
DIN 53504, S2
Tear Strength 20.0 kN/m114 pliDIN ISO 34-1
Compression Set  23 %
@Temperature 100 °C,
Time 252000 sec
23 %
@Temperature 212 °F,
Time 70.0 hour
DIN ISO 815, B
 45 %
@Temperature 150 °C,
Time 605000 sec
45 %
@Temperature 302 °F,
Time 168 hour
DIN ISO 815, B
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9377 / 293896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.