MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Vandar® 9118 Unfilled Polyester Alloy
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Description: Vandar 9118 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is typically used for unpainted cover/container applications

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183 & ASTM D792
Water Absorption <= 0.40 %ASTM D570
Linear Mold Shrinkage 0.015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1900 psiASTM D638
Elongation at Break >= 310 %50 mm/min; ISO 527-2/1A
 >= 310 %ASTM D638
Tensile Modulus 0.0700 GPa1 mm/min; ISO 527-2/1A
 10000 psiASTM D638
 2500 psi
@Temperature 85.0 °C
ASTM D638
 26000 psi
@Temperature -40.0 °C
ASTM D638
50% Modulus 0.0120 GPa
@Strain 50 %
ISO 527-2/1A
Flexural Strength 3.00 MPaISO 178
Flexural Yield Strength 520 psiASTM D790
Flexural Modulus 0.110 GPaISO 178
 12500 psiASTM D790
 27775 psiASTM D790
Izod Impact, Notched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Izod Impact, Notched (ISO) NBISO 180/1A
 NB
@Temperature -30.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 175 - 200 °C
Middle Barrel Temperature 185 - 205 °C
Front Barrel Temperature 190 - 215 °C
Nozzle Temperature 195 - 215 °C
Melt Temperature 190 - 215 °C
Mold Temperature 20.0 - 50.0 °C
Drying Temperature 175 - 220 °F
Dry Time 4 hour
Back Pressure 0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Vandar® AB700 High Modulus Polyester Alloy
Celanese Hytrel® 8238 TPC-ET
Chi Mei Polylac® PA-756 ABS - High Flow
Chi Mei Polylac® PA-726 ABS
AlphaGary Garathane™ X 94-350-B UV-DG2 Polyurethane based compound

PHCW62 / 46003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.