MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® R197 Magnesium Raspings
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Elektron® magnesium raspings have a coarse shape to provide maximum surface area and reactivity. Different lengths, widths and thickness can be supplied. The attached information sheets give details on our standard products. However, Magnesium Elektron are able to custom manufacture all products to your specific needs. We are also able to manufacture a product according to your sample or specification. Our production processes allow us to supply a high quality, consistent product. All our rasping products can be supplied in either standard or high purity grade. Elektron® raspings are typically used in the formation of Grignard reagents, for the synthesis of complex organic compounds in the pharmaceutical, chemical, plastics, and agricultural industries. Raspings possess a large surface area, which helps to control the vigorous nature of the reaction. Other areas of application include catalysts for resins, flavors and fragrances.

Information provided by Magnesium Elektron.

Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 g/cc0.0145 lb/in³Pour Density
Particle Size <= 212 µm<= 212 µmSieve Analysis: 1% max pass
 212 µm212 µmSieve Analysis: 99% min retained
 2800 µm2800 µmSieve Analysis: 0.1% max retained

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZA (K1A) Magnesium Zirconium Alloy
Magnesium Elektron Elektron® R418 Magnesium Raspings
Magnesium Elektron Elektron® R286 Magnesium Raspings
Magnesium Elektron Elektron® R176 Magnesium Raspings
Magnesium Elektron Elektron® AZ80A Magnesium Alloy, UNS M11800

NMAGEL920 / 186935

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.