MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Freudenberg Sealing Technologies Simriz Simtiz 485 (FFKM) Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Simriz has chemical stability similar to that of PTFE combined with the rubbery-elastic qualities of an elastomer. They are used wherever extreme safety standards are in force and high maintenance and repair expenditures exceed the costs of the seals.

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7676ASTM D2240
Tensile Strength 18.5 MPa2680 psiASTM D1414
Elongation at Break 195 %195 %ASTM D1414
100% Modulus 5.70 MPa827 psiASTM D1414
Compression Set  23 %
@Temperature 200 °C,
Time 252000 sec
23 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395 Method B
 31 %
@Temperature 200 °C,
Time 1.80e+6 sec
31 %
@Temperature 392 °F,
Time 500 hour
ASTM D395 Method B
 40 %
@Temperature 200 °C,
Time 3.60e+6 sec
40 %
@Temperature 392 °F,
Time 1000 hour
ASTM D395 Method B
 45 %
@Temperature 250 °C,
Time 252000 sec
45 %
@Temperature 482 °F,
Time 70.0 hour
ASTM D1414
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9343 / 293872

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.