MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes: Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.

Films obtained from Clearflex H&T FHH 508 show good optical properties, high rigidity, high temperature resistance and excellent sealing properties.

Main Applications: For its excellent optical properties and sealing performance, together with a very low gel content, Clearflex H&T FHH 508, is the ideal choice for the production of lamination films. Due to its softening point, Clearflex H&T FHH 508 is especially recommended for flexible packaging that have to withstand heat cycles such as cook-in films.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.935 g/ccISO 1183
Thickness 10.0 - 50.0 micronsRecommended
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 16.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPaISO 527-3
Film Elongation at Break, MD 600 %ISO 527-3
Film Elongation at Break, TD 900 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 3.057 g/micronISO 6383-2
Elmendorf Tear Strength, TD 13.247 g/micronISO 6383-2
Dart Drop Test 70.0 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 40.0 MPaISO 527-3
1% Secant Modulus, MD 430 MPaISO 527-3
1% Secant Modulus, TD 500 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 127 °CInternal method
Vicat Softening Point 117 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 13 %ISO 14782
Gloss 60 %45°; ASTM D2457
Transmission, Visible 90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENG063 / 124457

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.