MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.

Films obtained from Clearflex H&T LGH 108 have excellent optical properties, a wide sealing window, both hot tack and hot seal, together with a low sealing initiation temperature (S.I.T.) and outstanding impact, puncture and Elmendorf tear resistance.

Main Applications: Clearflex H&T LGH 108, for its overall characteristics, is the right choice for packaging film applications, bioriented film requiring superior mechanical and optical properties. Moreover, the excellent sealability behavior together with low gel content makes it ideal for lamination film production.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.917 g/ccISO 1183
Thickness 10.0 - 50.0 micronsRecommended
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 9.00 MPaISO 527-3
Film Tensile Strength at Yield, TD 9.00 MPaISO 527-3
Film Elongation at Break, MD 450 %ISO 527-3
Film Elongation at Break, TD 700 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 13.247 g/micronISO 6383-2
Elmendorf Tear Strength, TD 21.399 g/micronISO 6383-2
Dart Drop Test 400 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPaISO 527-3
Film Tensile Strength at Break, TD 45.0 MPaISO 527-3
1% Secant Modulus, MD 160 MPaISO 527-3
1% Secant Modulus, TD 170 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 117 °CInternal method
Vicat Softening Point 102 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %ISO 14782
Gloss 60 %45°; ASTM D2457
Transmission, Visible 90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem LL5800N LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
Borealis Borstar® FB2310 LLDPE for Film
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin

PENG077 / 124471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.