MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Orthoclase (Feldspar KAlSi3O8)
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Two cleavage directions. Weathering end products: Kaolinite illite. An important rock forming mineral occurring in basic igneous (granite, syeite, granodiorite) and metamorphic. All feldspars are good indicators of the rock freshness.

Property values are typical of naturally occurring Orthoclase (Feldspar KAlSi3O8). Actual property values will vary from sample to sample.

Key Words: KAlSi3O8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.57 g/cc0.0928 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 560560
Hardness, Vickers 714714
Hardness, Mohs 6.06.0
Abrasive Hardness 3737
Drilling Hardness 46654665
 
Thermal PropertiesMetricEnglishComments
CTE, linear  2.80 µm/m-°C
@Temperature 20.0 - 200 °C
1.56 µin/in-°F
@Temperature 68.0 - 392 °F
calculated from volumetric expansion
 5.20 µm/m-°C
@Temperature 20.0 - 500 °C
2.89 µin/in-°F
@Temperature 68.0 - 932 °F
calculated from volumetric expansion
 
Descriptive Properties
ColorWhite and Red

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Albite (Plagioclase Feldspar NaAlSi3O8)
Mica (KAl2(AlSi3O10)(OH)2)
Borosilicate Glass
Feldspar (K2O-Al2O3-6SiO2)
Muscovite (KAl2(AlSi3O10)-(OH)2)

BMIN104 / 220

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.