MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess LEWATIT® MonoPlus MP 64 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus MP 64 is a weakly basic, macroporous anion exchange resin with beads of uniform size (monodisperse) based on a styrene-divinylbenzene copolymer. The monodisperse beads are chemically and osmotically highly stable. The optimized kinetics lead to an increased operating capacity compared to ion exchange resins with heterodisperse bead size distribution. Lewatit MonoPlus MP is especially applicable for:
  • the demineralization of water for industrial steam generation in combination with strong basic ion exchangers like Lewatit MonoPlus M 500 (particularly for water with a high loading of humic acids and other organic substances) especially recommended for Lewatit WS System
  • the treatment of electroplating rinse waters
  • the demineralization of water with a high concentration of humic acids and other organic substances to protect the strong basic anion exchanger from fouling
Lewatit MonoPlus MP 64 adds special features to the resin bed:
  • high exchange flow rates during regeneration and loading
  • an excellent utilization of the total capacity
  • a low demand for rinse water
  • homogenous throughput of regenerates, water and solutions; therefore a homogeneous working zone
  • a nearly linear pressure drop gradient for the whole bed depth; therefore an operation with higher bed depth possible

    Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density 1.04 g/cc0.0376 lb/in³
Bead Size 0.540 - 0.640 mm0.0213 - 0.0252 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBeige, opaque
pH Operating Range0 - 7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8786 / 209178

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.