MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Apcotex Apcotex TY100 Styrene Butadiene Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Apcotex TY100 is a copolymer of styrene butadiene latex used for dipping of fabric for tyre cord, V-belts and conveyor belts. Its application also includes textile finishing and adhesive. It is manufactured by emulsion polymerization method with state-of-the-art manufacturing facilities to produce consistent product.

Advantages:

  • Excellent Mechanical stability and chemical stability
  • Compatible with vinyl pyridine latex
  • Aids in processing
  • Excellent gloss development and good wet pick resistance
  • Good tackiness properties
  • Provide excellent film strength

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 - 42 %
pH 10 - 12
Brookfield Viscosity 20 - 60 cPLVF, SP.1, 60 RPM
Mooney Viscosity <= 90
@Temperature 100 °C
ML 1+4; ASTM D1417
Surface Tension 54 - 64 dynes/cm
Storage Temperature 5.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceOff white liquid
Content<0.05%Coagulum
Emulsifying SystemSynthetic anionic
Mechanical stability<0.3 g/100cc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPCOT060 / 315639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.