MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Opti-Polymers Optimid PA6 GF10 GK20 V0/1,6mm PA6, 10% Glass Fiber Filled and 20% Glass Pearls Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Glass Bead Filled

Material Notes: Reinforced, flame retardant PA6 compound with low warping tendency and low shrinkage. Injection moulding. Different colors available.

Information provided by Opti-Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Maximum Moisture Content 0.20
@Temperature 120 °C,
Time 299 sec
0.20
@Temperature 248 °F,
Time 0.0830 hour
thermogravimetric
Ash 18 - 22 %
@Temperature 625 °C
18 - 22 %
@Temperature 1160 °F
ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 85.0 MPa
@Time 86400 sec
12300 psi
@Time 24.0 hour
5 mm / min, 50% RH; ISO 527-1
Elongation at Break 2.5 %
@Time 86400 sec
2.5 %
@Time 24.0 hour
5 mm / min, 50% RH; ISO 527-1
Tensile Modulus 7.00 GPa
@Time 86400 sec
1020 ksi
@Time 24.0 hour
1 mm / min, 50% RH; ISO 527-1
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FISO75-1/-2
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
DIN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °Finjection molding
Mold Temperature 60.0 - 85.0 °C140 - 185 °Finjection molding
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Regional AvailabilityEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POPTI005 / 255141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.