Hostacom TRC 787N C4 high melt flow mineral-filler filled thermoplastic elastomeric olefin(TEO) resin has an excellent balance of processability, rigidity, and impact and scratch and mar resistance. It can be used for automotive interior applications, such as instrument panel, console, glove box. This grade can be colored, pellet form. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Asia-Pacific Application: Instrument Panels; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Good Colorability; Good Moldability; High Flow; High Impact Resistance; High Stiffness; Scratch Resistant Information provided by LyondellBasell. |