MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lord Adhesives Circalok™ 6403 A SLW/B Urethane Encapsulant System
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: LORD Circalok™ 6403 A SLW/B urethane encapsulant is a general purpose, two-component urethane designed for applications requiring a fast cure, mechanical shock-resistant system. Circalok 6403 A SLW/B urethane encapsulant does not contain MOCA or TDI.

Features: maintains low viscosity for complete and void-free encapsulation. provides excellent protection and resistance to moisture; exhibits excellent hydrolytic stability. provides excellent electrical insulation properties. can be used on parts and devices that experience operating temperatures from -50°C to +120°C.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/cc6403 A SLW Resin
 1.04 g/cc1.04 g/ccMixed
 1.19 g/cc1.19 g/cc6403 B Hardener
Viscosity  750 cP
@Temperature 27.0 °C
750 cP
@Temperature 80.6 °F
6403 A SLW Resin
 900 cP
@Temperature 27.0 °C
900 cP
@Temperature 80.6 °F
Mixed
 1200 cP
@Temperature 27.0 °C
1200 cP
@Temperature 80.6 °F
6403 B Hardener
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080cured
Tensile Strength 13.34 MPa1935 psicured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 ohm-cm
@Temperature 77.0 °F
cured; ASTM D 257
Dielectric Constant 3.6
@Frequency 1000 Hz,
Temperature 25.0 °C
3.6
@Frequency 1000 Hz,
Temperature 77.0 °F
cured
Dielectric Strength 23.6 kV/mm600 kV/incured
Dissipation Factor 0.14
@Frequency 1000 Hz,
Temperature 25.0 °C
0.14
@Frequency 1000 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 10.0 - 15.0 min10.0 - 15.0 minmixed
Shelf Life 6.00 Month
@Temperature 25.0 - 40.0 °C
6.00 Month
@Temperature 77.0 - 104 °F
each component from date of manufacture
 
Descriptive Properties
AppearanceAmber Liquid6403 A SLW Resin
 Amber Liquid6403 B Hardener
 Amber LiquidMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9265 / 232621

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.