MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Huntsman KRYSTALFLEX® PE 399 (Colored) Polyurethane Optical Aliphatic Film
Categories: Polymer; Film; Thermoplastic; Polyurethane, TP

Material Notes: Key Properties:
  • Moisture Resistance
  • Chemical Compatibility
  • Cooler Processing
  • Higher Adhesion
  • Multiple Design Option
  • No special storage required

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength at Break 4000 - 5600 psiASTM D412
Elongation at Break 380 - 400 %ASTM D412
100% Modulus 0.260 - 0.390 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.70 - 2.20 ksi
@Strain 300 %
ASTM D412
Tear Strength 240 - 280 pliASTM D624
Peel Strength 45.0 - 85.0 pli
@Temperature 91.0 °C
resistance to glass; ASTM D3167
 112 - 123 pli
@Temperature 99.0 °C
resistance to glass; ASTM D3167
 126 - 148 pli
@Temperature 113 °C
resistance to glass; ASTM D3167
 136 - 140 pli
@Temperature 118 °C
resistance to glass; ASTM D3167
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -36.0 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 76.0 - 140 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman KRYSTALFLEX® PE 900 Polyurethane Optical Aliphatic Film
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film

PHUQ131 / 159504

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.