MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP

Material Notes: Superior Chemical Resistance, Impact Modified

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Linear Mold Shrinkage 0.013 - 0.018 cm/cmASTM D955
Melt Flow 6.0 - 12 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6150 psiASTM D638
Tensile Strength, Yield 6150 psiASTM D638
Flexural Strength 9100 psiASTM D790
Flexural Modulus 250 ksiASTM D790
Izod Impact, Notched 8.00 ft-lb/in
@Temperature -34.4 °C
ASTM D256
 16.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
 HB
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 440 - 470 °F
Middle Barrel Temperature 450 - 480 °F
Front Barrel Temperature 460 - 500 °F
Melt Temperature 460 - 500 °F
Mold Temperature 120 - 180 °F
Drying Temperature 220 - 230 °F
Dry Time 4.00 - 6.00 hour
Vent Depth 0.00150 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 50015 PET, Pellet, Injection Molded Natural Color
Plenco 50015 PET, Pellet, Injection Molded, White
Eastman Eastar GN101 PETG Copolyester
Eastman Eastar GN007 PETG Copolyester
Eastman Aqua WA314 PET

PPOLYQ108 / 160624

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.