Key features:- 100% solid content
- Good chemical resistance
- Good hydrolysis resistance
- Yellowing resistance
- High bonding performance
- Solvent-free Eco-friendly
Application: This PUR hot melt can be used for fabric/fabric, fabric /TPU film lamination.Information provided by Taiwan PU Corporation |