MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Silon PA 0835 HD Processing Aid Concentrate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Masterbatch with a highly effective processing aid for polyethylene, especially PE-HD. By using the PA 0835 HD, the output can be markedly increased and the pressure build-up in the barrel decreased without increasing the screw speed. The result is an increase of the screw lifetime. PA 0835 HD prevents the build-up of deposits in the die that are caused by high pigment concentration (titanium dioxide), flame retardant, and blowing agents. Blown hollow articles from PE-HD types with different densities will get a markedly improved surface by the dosage of PA 0835 HD.

Information provided by Silon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.550 g/cc
Density 0.980 g/cc
Volatiles <= 0.25 %
Melt Flow 7.62 g/10 min
@Load 2.16 kg,
Temperature 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILON45 / 83583

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.