Hostacom EKG 2087T LW C12A22 is a 30% glass fiber reinforced PP (coupled). It combines excellent stiffness properties with good dimensional stability and low creep under load at elevated temperatures. This grade is delivered in (laser transparent) black color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |