MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Aremco’s Corr-Paint™ epoxy and urethane-based coatings are used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag houses, cyclones, hoppers and other process equipment used in the power, pulp and paper, and chemical processing industries.

Features

  • Single-Part, No Mixing
  • Low Viscosity
  • Cures at Room Temperature
  • High Wear Resistance
  • Excellent Salt Spray Resistance
  • Maximum Temperature, 400 °F

Key Words: High Temperature Coatings
Vendors: Aremco’s Corr-Paint™ epoxy and urethane-based coatings are used for producing corrosion and wear resistant barriers. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag houses, cyclones, hoppers and other process equipment. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
Solids Content 66 %volume
 70 %weight
Volatile Organic Compounds (VOC) Content 359.5 g/l
Viscosity 300 - 600 cPMixed Viscosity
Thickness 2.60 milrecommended dry film thickness
 4.00 milestimated wet film thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Flash Point 140 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Dry Time 4.00 - 6.00 hourTouch
 6.00 - 8.00 hourHandling
 6.00 - 12.0 hourRecoat
Cure Time 1.00 hour
@Temperature 121 °C
>1 Hour Air Set Required Prior to Curing
 24.0 hour
@Temperature 22.2 °C
>1 Hour Air Set Required Prior to Curing
Shelf Life 12.0 Month
@Temperature 23.0 °C
 
Descriptive Properties
ColorAluminum
Dry Film Coverage ft2/gal1058at 1 mil
PrimerNot Required or Recommended
ThinnerHi-Flash Naphtha

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese 50000455 Ethyl Acetate
Evonik VISIOMER® Terra C13-MA Methacrylate Monomer
Evonik VISIOMER® c-HMA Methacrylate Monomer
Celanese 51002165 Ethyl Acetate Kosher Grade
Celanese 50000429 Crotonaldehyde

CAREM67 / 608

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.