MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ExxonMobil ESCOREZ™ 2596 Petroleum Hydrocarbon Resin  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Adhesive

Material Notes: Light colored, premium, aromatic modified aliphatic resin. It is designed to tackify a variety of adhesive polymers including EVA, APP, APAO, SIS block copolymers, natural rubber, synthetic polyisoprene, polyisobutylene and butyl rubber.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
@Temperature 20.0 °C
20/20°C (IPOH); ETM 22-28
Brookfield Viscosity 4000 cP
@Temperature 140 °C
ETM 22-31
Molecular Weight 780 g/molMn; ETM 300-83
 1700 g/molMw; ETM 300-83
 3600 g/molMz; ETM 300-83
Ash <= 0.10 %ETM 22--05
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0mg KOH/g; ETM 22-49
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 45.0 °CETM 300-90
Ring & Ball Softening Point 96.0 °CETM 22-24
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 2.0Initial; ETM 22-13
 4.5Molten; ETM 22-12
 8.0Aged for 16 hours @ 300°F; ETM 22-15
 
Descriptive Properties
Chloride Content, ppm400

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Gallium Arsenide Semiconductor Wafer, n-type, Silicon Doped, HB-GF Grown
Arkema OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
AGC F-Clean® GR 80
Parker Chomerics CHO-SHIELD® 576 Part B Coating Catalyst
Overview of materials for Low Density Polyethylene (LDPE), Film Grade

PEXB498 / 37803

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.