MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cronifer 18-15 LCSi Austenitic Stainless Steel Annealed Plate, Sheet, Strip, UNS S30600
Categories: Metal; Ferrous Metal; Stainless Steel; T S30000 Series Stainless Steel

Material Notes:

Information provided by Industeel, ATI, and the references(s).

Key Words: ASTM A 240, Cronifer 1815 LCSi
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 540 MPa78300 psi
Tensile Strength, Yield 240 MPa34800 psi
Elongation at Break 40 %40 %
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.220.22Calculated
Shear Modulus 82.0 GPa
@Temperature 20.0 °C
11900 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000750 ohm-cm0.0000750 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.5 µm/m-°C
@Temperature 20.0 - 100 °C
9.17 µin/in-°F
@Temperature 68.0 - 212 °F
 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
 19.0 µm/m-°C
@Temperature 20.0 - 500 °C
10.6 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.200 J/g-°C0.0478 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.018 %<= 0.018 %
Chromium, Cr 17 - 18.5 %17 - 18.5 %
Iron, Fe 59.442 - 65.3 %59.442 - 65.3 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.20 %<= 0.20 %
Nickel, Ni 14 - 15.5 %14 - 15.5 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 3.7 - 4.3 %3.7 - 4.3 %
Sulfur, S <= 0.020 %<= 0.020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Crucible Steel CPM® S90V® (420V®) Tool Steel
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 0% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200)

MQZ9913 / 172121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.